Comparative Electrochemical Noise Characterization of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V in Ringer’s Solution Using Statistical and Hilbert–Huang Analyses
Gaona Tiburcio, Citlalli y Maldonado Bandala, Erick y Jáquez Muñoz, Jesús Manuel y Nieves Mendoza, Demetrio y Méndez Ramírez, Ce Tochtli y Almeraya Gaona, Bruno y Landa Ruiz, Laura y Baltazar García, Brenda Paola y Estupiñan López, Francisco Humberto y Jáquez Muñoz, Jesús Manuel y López León, Luis Daimir y Olguín Coca, Javier y Almeraya Calderón, Facundo (2026) Comparative Electrochemical Noise Characterization of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V in Ringer’s Solution Using Statistical and Hilbert–Huang Analyses. Materials, 19 (20). pp. 1-20. ISSN 1996-1944
|
Texto
materials-19-04337.pdf - Versión Publicada Available under License Creative Commons Attribution Non-commercial No Derivatives. Download (3MB) | Vista previa |
Resumen
Titanium and its alloys are widely used in biomedical applications because of their favorable mechanical properties, biocompatibility, and corrosion resistance. This study comparatively evaluated the electrochemical behavior of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V in Ringer’s solution using electrochemical noise (EN), empirical mode decomposition (EMD), Hilbert–Huang Transform (HHT), and scanning electron microscope/Energy-dispersive X-ray spectroscopy (EDS) SEM/EDS characterization. Statistical EN analysis revealed marked differences among the investigated materials. Ti-6Al-2Sn-4Zr-2Mo exhibited the highest noise resistance (45,412 ± 57 Ω·cm2), followed by Ti-6Al-4V (11,784 ± 39 Ω·cm2) and Ti-CP2 (4114 ± 45 Ω·cm2), whereas relatively low localization index values were obtained for all three materials (0.02634–0.06). EMD revealed four, five, and six intrinsic mode functions for Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V, respectively. Hilbert time–frequency–amplitude analysis further demonstrated distinct temporal and frequency distributions of the electrochemical fluctuations, with Ti-6Al-4V exhibiting the broadest and most persistent distribution of transient activity. SEM/EDS revealed localized post-exposure compositional heterogeneity and different degrees of accumulation of electrolyte-derived species but was not interpreted as direct evidence of passive-film chemistry or integrity. Overall, the combined statistical EN, EMD, Hilbert time–frequency, and SEM/EDS results demonstrate distinct passive electrochemical responses among the three titanium materials, with Ti-6Al-2Sn-4Zr-2Mo exhibiting the highest resistance to electrochemical fluctuations under the investigated conditions.
| Tipo de elemento: | Article | ||||||||||||||||||||||||||||||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Palabras claves no controlados: | Titanium alloys, Ti-CP2, Electrochemical noise, Hilbert–Huang transform, Empirical mode decomposition, Ringer’s solution, SEM/EDS | ||||||||||||||||||||||||||||||||||||||||||
| Materias: | CONACYT > Ingeniería y Tecnología Q Ciencia > Q Ciencias en General Q Ciencia > QD Química T Tecnología > TL Vehículo Motor, Aeronáutica, Astronáutica T Tecnología > TN Ingeniería Minera. Metalurgia |
||||||||||||||||||||||||||||||||||||||||||
| Divisiones: | Ingeniería Mecánica y Eléctrica > Doctorado en Ciencias de la Ingeniería Aeronáutica | ||||||||||||||||||||||||||||||||||||||||||
| Usuario depositante: | Dra Citlalli Gaona | ||||||||||||||||||||||||||||||||||||||||||
| Creadores: |
|
||||||||||||||||||||||||||||||||||||||||||
| Fecha del depósito: | 24 Nov 2026 15:06 | ||||||||||||||||||||||||||||||||||||||||||
| Última modificación: | 24 Nov 2026 15:06 | ||||||||||||||||||||||||||||||||||||||||||
| URI: | http://eprints.uanl.mx/id/eprint/31910 |
Actions (login required)
![]() |
Ver elemento |
orcid.org/0000-0001-9072-3090
Descargar estadísticas
Descargar estadísticas